Thermal cyclic test for Sn-4Ag-0.5Cu solders on high P Ni/Au and Ni/Pd/Au surface finishe

Authors

  • M.A. Azmah Hanim Department of Mechanical and Manufacturing Engineering, Faculty of Engineering, Universiti Putra Malaysia, 43400 Serdang, Selangor, Malaysia
  • A. Ourdjini Faculty of Mechanical Engineering, Universiti Teknologi Malaysia, 81310 Skudai, Johor, Malaysia
  • I. Siti Rabiatull Aisha Faculty of Mechanical Engineering, Universiti Malaysia Pahang, 26600 Pekan, Pahang, Malaysia
  • O. Saliza Azlina Faculty of Mechanical & Manufacturing Engineering, Universiti Tun Hussein Onn Malaysia, 86400 Batu Pahat, Johor, Malaysia

DOI:

https://doi.org/10.15282/jmes.9.2015.4.0152

Keywords:

Ni/Au; Ni/Pd/Au; lead free solders, thermal cyclic test; Sn-4Ag-0.5Cu.

Abstract

In electronic packaging, the reliability of the interconnection changes with the surface finish and the type of solders being used. Thermal cycling is one method of reliability assessment. In thermal cycling experiments, the strain state is simplified by soldering together regular shaped pieces of materials with different coefficients of thermal expansion and exposing the joint to repeated fluctuations of temperature within a certain range. Thus, this study focuses on the intermetallic evolution of Sn-4Ag-0.5Cu on Ni/Au and Ni/Pd/Au surface finishes with thermal cycling up to 1000 cycles with the range of temperature varying from 10 to 80 °C. Sandwich samples were prepared by placing solder balls of Sn-4Ag-0.5Cu between two substrates of two different surface finishes: Ni/Au and Ni/Pd/Au. Optical microscope and FESEM (Field emission scanning electron microscope) were used to analyze the samples. From the study, it was observed that the intermetallic changes from (Cu, Ni)6Sn5 to (Ni, Cu)3Sn4 after 1000 thermal cycles for Ni/Au. These changes promote the formation of cracks at the solder joint because of the different mechanical properties between Ni-Sn based intermetallic and Cu-Sn intermetallics. However, for the Ni/Pd/Au surface finishes, no cracks formed after thermal cycling up to 1000 cycles. This shows that the reliability of the solder joint is higher for Ni/Pd/Au surface finishes in this experiment. Based on these results, it can be concluded that the reliability of the Ni/Pd/Au surface finishes with Sn-4Ag-0.5Cu solders is higher within the given condition of this research.

References

Kim B-K, Lee S-J, Kim J-Y, Ji K-Y, Yoon Y-J, Kim M-Y, et al. Origin of surface defects in PCB final finishes by the electroless nickel immersion gold process. Journal of Electronic Materials. 2008;37:527-34.

Kim J-H, Lee Y-C, Lee S-M, Jung S-B. Effect of surface finishes on electromigration reliability in eutectic Sn–58Bi solder joints. Microelectronic Engineering. 2014;120:77-84.

Coombs CF. Coombs' printed circuits handbook: McGraw-Hill Professional Publishing; 2001.

Harper C. Electronic packaging and interconnection handbook: McGraw-Hill, Inc.; 2004.

Zhang L, Sun L, Guo Y-h, He C-w. Reliability of lead-free solder joints in CSP device under thermal cycling. Journal of Materials Science: Materials in Electronics. 2014;25:1209-13.

Ma H, Suhling JC. A review of mechanical properties of lead-free solders for electronic packaging. Journal of Materials Science. 2009;44:1141-58.

Siti Rabiatull Aisha I, Hanim A, Ariff M, Ourdjini A, Saliza Azlina O. Intermetallic evolution for isothermal aging up to 2000 hours on Sn-4ag-0.5 cu and Sn-37pb Solders with Ni/Au Layers. International Journal of Automotive and Mechanical Engineering. 2013;8:1348-56.

Hanim M, Ourdjini A, Aisha I, Azlina OS. Effect of isothermal aging 2000 hours on intermetallics formed between Ni-Pd-Au with Sn-4Ag-0.5 Cu solders. Advanced Materials Research. 2013; 650: 194-9.

Labie R, Ruythooren W, Van Humbeeck J. Solid state diffusion in Cu–Sn and Ni– Sn diffusion couples with flip-chip scale dimensions. Intermetallics. 2007;15:396- 403.

Jang J, Frear D, Lee T, Tu K. Morphology of interfacial reaction between lead- free solders and electroless Ni–P under bump metallization. Journal of Applied Physics. 2000;88:6359-63.

Huang Z, Conway PP, Jung E, Thomson RC, Liu C, Loeher T, et al. Reliability issues in Pb-free solder joint miniaturization. Journal of Electronic Materials. 2006;35:1761-72.

George E, Das D, Osterman M, Pecht M. Thermal cycling reliability of lead-free solders (SAC305 and Sn3. 5Ag) for high-temperature applications. IEEE Transactions on Device and Materials Reliability. 2011;11:328-38.

Downloads

Published

2015-12-31

How to Cite

[1]
M. . Azmah Hanim, A. . Ourdjini, I. . Siti Rabiatull Aisha, and O. . Saliza Azlina, “Thermal cyclic test for Sn-4Ag-0.5Cu solders on high P Ni/Au and Ni/Pd/Au surface finishe”, J. Mech. Eng. Sci., vol. 9, pp. 1572–1579, Dec. 2015.