Mechanical Behavior of Hybrid Laminated Nano Composite Containing Equal Numbers of Glass and Carbon Fiber Plies

Authors

  • Ava A.K. Mohammed Department of Technical Mechanical and Energy Engineering, Erbil Technical Engineering College, Erbil Polytechnic University, 44001 Erbil, Iraq https://orcid.org/0000-0002-3658-0014
  • Gailan Ismail Hassan Department of Technical Mechanical and Energy Engineering, Erbil Technical Engineering College, Erbil Polytechnic University, 44001 Erbil, Iraq https://orcid.org/0000-0003-2472-4612
  • Younis Khalid Khdir Department of Technical Mechanical and Energy Engineering, Erbil Technical Engineering College, Erbil Polytechnic University, 44001 Erbil, Iraq https://orcid.org/0000-0001-5861-1283

DOI:

https://doi.org/10.15282/ijame.20.2.2023.01.0799

Keywords:

Glass/Carbon hybrid, Nano-Al2O3, VARIM, Cross laminates, Quasi laminates

Abstract

Hybrid fiber reinforced polymer with nanofiller composite was introduced into a lot of industries due to its extreme mechanical properties in comparison with non-hybrid material. In this investigation, cross and quasi-fiber laminated epoxy composites with and without nano Al2O3 were fabricated using Vacuum Assisted Resine Infusion Method and Ultrasonic Dual Mixing Method. In general, the results of mechanical properties indicated that the addition of 2% nano Al2O3 enhances the tensile and flexural properties. Cross number 2 with nano Al2O3 laminate had the maximum tensile strength 628 MPa and maximum tensile strain of 1.74%, while cross number 1 with nano Al2O3 laminate had the maximum tensile modulus of 37.756 GPa in the cross group. In the quasi group, quasi number 2 with nano Al2O3 had the maximum tensile strength, maximum tensile strain, and maximum tensile modulus, equal to 294 MPa, 1.98%, and 16.409 GPa, respectively. Regarding the flexural properties, cross number 1 with nano Al2O3 laminate had a maximum flexural strength of 708.2 MPa and maximum flexural strain of 2.027%, while cross number 2 with nano Al2O3 laminate had a maximum flexural modulus of 38.73 GPa in the cross group. On the other hand, quasi number 1 with nano Al2O3 laminate had the maximum flexural strength, maximum flexural strain, and maximum flexural modulus equal to 596 MPa, 2.424%, and 29.2 GPa, respectively in the quasi group. The internal structures of the failure laminated composites through scanning electronic microscopy confirm that the adhesion between fibers and matrix is good.

Downloads

Published

2023-06-30

How to Cite

[1]
Ava Mohammed, Gailan Ismail Hassan, and Younis Khalid Khdir, “Mechanical Behavior of Hybrid Laminated Nano Composite Containing Equal Numbers of Glass and Carbon Fiber Plies ”, Int. J. Automot. Mech. Eng., vol. 20, no. 2, pp. 10335–10350, Jun. 2023.

Issue

Section

Articles

Similar Articles

1 2 3 4 5 6 7 8 9 10 > >> 

You may also start an advanced similarity search for this article.